MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Niobium Carbide, NbC
Categories: Ceramic; Carbide

Material Notes: Gray cubic crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.60 g/cc0.275 lb/in³typical processed
 7.82 g/cc0.283 lb/in³theoretical
Molecular Weight 104.917 g/mol104.917 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 9090at RT
Vickers Microhardness 24002400
Tensile Strength, Ultimate 244 MPa35400 psiat RT
Modulus of Elasticity 330 - 537 GPa47900 - 77900 ksi
Compressive Strength 2374 MPa344300 psiat RT
Poissons Ratio  0.22
@Temperature 23.0 °C
0.22
@Temperature 73.4 °F
 0.25
@Temperature 1930 °C
0.25
@Temperature 3510 °F
Shear Modulus 197 - 245 GPa28600 - 35500 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000740 ohm-cm0.0000740 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.70 µm/m-°C
@Temperature 20.0 °C
3.72 µin/in-°F
@Temperature 68.0 °F
Melting Point 3500 °C6330 °F
Solidus 3425 °C6197 °F
Liquidus 3575 °C6467 °F
Boiling Point 4300 °C7770 °F
 
Descriptive Properties
CAS Number12069-94-2
ColorGray
Crystal StructureCubicNaCl Structure

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Carbide, TiC
Zirconium Carbide, ZrC
Tantalum Carbide, TaC
Tungsten Carbide, WC
Goodfellow Vycor® 7913 Glass

BCNC1A / 158

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.