MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

W. L. Gore GORE™ 800 PTFE Universal Pipe Gasket (Style 800)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: 100% expanded PTFE, with multi-directional strength. Resistant to all media in the 0-14 pH range, except molten alkali metals and element fluorine, particularly at elevated temperatures and pressures. Complies with FDA 21 CFR 177.1550 (PTFE) food requirements.

GORE Universal Pipe Gaskets are used to seal all types of flanges in chemical-process piping. Style 800 gaskets are designed to meet the needs of various piping materials. They are ideal for standardizing gasket material across steel, glass-lined steel, and FRP systems -- any application in which a non-metallic gasket can be used.

Key Features:

  • 100 percent expanded PTFE
  • Chemically inert and temperature resistant
  • Seals at low bolt load
  • Conforms to flange deviations
  • High dimensional stability
  • Resists creep and cold flow
  • Resistant to blowout
Key Benefits:
  • Seals all types of standard piping
  • Standardize: One gasket system-wide
  • Protects against use of wrong gasket
  • Lowers process emissions
  • Reliable sealing performance
  • Seldom needs retorquing
  • Lowers total sealing cost

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 316 °C600 °F
Minimum Service Temperature, Air -268 °C-450 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Compressibility57%ASTM F36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsamid® AESNO MED Nylon 12
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Saint-Gobain Chemfab® 5 Anti-Static PTFE-Coated Glass
Overview of materials for Acetal Homopolymer, PTFE-Filled
3M Dyneon™ TF 2021 PTFE

PGORE00 / 42293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.