MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® B3 3 S3 10 natural PA 6 Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Description: AKROMID B3 3 S3 10 natural is a nonreinforced, nucleated, dry impact resistant polyamide 6 with light inherent color. Applications are handles and fittings for power tools and furniture industry.

Additive: Nucleating Agent

Features:

  • Nucleated
Uses:
  • Fittings
  • Handles
  • Furniture
  • Power/Other Tools

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Moisture Absorption 2.6 %
@Temperature 70.0 °C
2.6 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.0 MPa5800 psi50 [mm/min]; ISO 527-2
Elongation at Break >= 100 %>= 100 %50 [mm/min]; ISO 527-2
Elongation at Yield 15 %15 %50 [mm/min]; ISO 527-2
Tensile Modulus 0.955 GPa139 ksi1 [mm/min]; ISO 527-2
Flexural Modulus 0.950 GPa138 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.80 J/cm²
@Temperature 23.0 °C
13.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 224 °C435 °FDIN EN 11357-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Akulon® K224-HG8 PA6-GF40, Conditioned, 40% Glass Filled, Heat Stabilized
Akro-Plastic Akromid® B3 S3 75 PA, Dry-Impact Resistant
Overview of materials for Nylon 6, Impact Grade
BASF Ultramid® 8253 PA6 (Dry)
BASF Capron® 8351 Impact Modified Nylon 6 (Dry)

PAKRO252 / 182839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.