MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem Green PE SHE150 High Density Polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Description: SHE150 resin is a High Density Polyethylene, copolymer of butene-1. It has been specially designed for monofilament extrusion process and provides a good balance of processability, spinnability, knotting strength as well as a very low gels amount. It can also be blended with LLDPE to improve blown film stiffness. It contains processing aid and antioxidant additives. The minimum biobased content of this grade is 94%, determined according to ASTM D6866.

Application: Raschel; shading and protecting nets; ropes.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ASTM D2240
Tensile Strength at Break 40.0 MPa5800 psiASTM D638
Tensile Strength, Yield 28.0 MPa4060 psiASTM D638
Flexural Modulus, 1% Secant 1280 MPa186000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C169 °FASTM D648
Vicat Softening Point 128 °C262 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Green PE SGD4960 Blow Molded High Density Polyethylene
Braskem Green PE SGF4950HS Blow Molded High Density Polyethylene
Braskem Green PE SHE150 Blown Film Extrusion and Cast Film Extrusion High Density Polyethylene
Braskem Green PE SEB853/72 Blown Film Extrusion Low Density Polyethylene
Braskem Green PE SEB853 Blown and Cast Film Extrusion Low Density Polyethylene

PBRASK2006 / 199888

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.