MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Petropol Nypol® B3 T10 TZ PRTA011 NT382 Nylon 6, 10% Mineral Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Mineral Filled

Material Notes: Product Description: 10% Mineral Reinforced, Polyamide 6

Resin ID (ISO 1043): PA6-MD10
Processing: Injection Molding
Color: Black

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %Humidity Absorption; ASTM D570
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inASTM D955
Ash 8.0 - 12 %8.0 - 12 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa13100 psiASTM D638
Elongation at Break 8.0 %8.0 %ASTM D638
Flexural Strength 90.0 MPa13100 psiASTM D790
Flexural Modulus 4.00 GPa580 ksiASTM D790
Izod Impact, Notched 0.500 J/cm0.937 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 - 225 °C428 - 437 °FASTM D2117
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 - 270 °C482 - 518 °FMolding
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 90.0 °C194 °F
Dry Time 3.00 hour3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL156 / 313064

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.