MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polypropylene with 30% Glass Fiber Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.60 g/cc0.0361 - 0.0578 lb/in³Average value: 1.14 g/cc Grade Count:539
Filler Content 25.0 - 33.0 %25.0 - 33.0 %Average value: 29.6 % Grade Count:136
Water Absorption 0.000 - 2.00 %0.000 - 2.00 %Average value: 0.0499 % Grade Count:71
Moisture Absorption at Equilibrium 0.0100 - 0.100 %0.0100 - 0.100 %Average value: 0.0460 % Grade Count:5
Water Absorption at Saturation 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.138 % Grade Count:4
Additive Loading 30.0 %30.0 %Average value: 30.0 % Grade Count:10
Maximum Moisture Content 0.0100 - 0.2000.0100 - 0.200Average value: 0.105 Grade Count:6
 0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.000600 - 0.0350 cm/cm0.000600 - 0.0350 in/inAverage value: 0.00401 cm/cm Grade Count:324
 0.00400 - 0.00400 cm/cm
@Temperature 80.0 - 80.0 °C
0.00400 - 0.00400 in/in
@Temperature 176 - 176 °F
Average value: 0.00356 cm/cm Grade Count:1
 0.00350 - 0.00350 cm/cm
@Temperature 220 - 240 °C
0.00350 - 0.00350 in/in
@Temperature 428 - 464 °F
Average value: 0.00356 cm/cm Grade Count:4
 0.00350 - 0.00350 cm/cm
@Pressure 60.0 - 60.0 MPa
0.00350 - 0.00350 in/in
@Pressure 8700 - 8700 psi
Average value: 0.00356 cm/cm Grade Count:4
Linear Mold Shrinkage, Transverse 0.000800 - 0.0193 cm/cm0.000800 - 0.0193 in/inAverage value: 0.00782 cm/cm Grade Count:99
 0.00800 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
0.00800 - 0.00800 in/in
@Temperature 176 - 176 °F
Average value: 0.00800 cm/cm Grade Count:1
Melt Flow 0.300 - 25.0 g/10 min0.300 - 25.0 g/10 minAverage value: 7.66 g/10 min Grade Count:404
Spiral Flow  95.0 - 95.0 cm
@Temperature 250 - 250 °C
37.4 - 37.4 in
@Temperature 482 - 482 °F
Average value: 95.0 cm Grade Count:1
 95.0 - 95.0 cm
@Thickness 2.00 - 2.00 mm
37.4 - 37.4 in
@Thickness 0.0787 - 0.0787 in
Average value: 95.0 cm Grade Count:1
Ash 26.0 - 34.0 %26.0 - 34.0 %Average value: 30.0 % Grade Count:26
 28.0 - 32.0 %
@Temperature 600 - 700 °C
28.0 - 32.0 %
@Temperature 1110 - 1290 °F
Average value: 30.0 % Grade Count:6
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 57.0 - 10757.0 - 107Average value: 66.7 Grade Count:9
Hardness, Rockwell R 81.0 - 11581.0 - 115Average value: 100 Grade Count:64
Hardness, Shore D 47.0 - 85.047.0 - 85.0Average value: 72.8 Grade Count:29
Ball Indentation Hardness 64.0 - 132 MPa9280 - 19100 psiAverage value: 111 MPa Grade Count:8
Tensile Strength, Ultimate 6.89 - 180 MPa1000 - 26100 psiAverage value: 81.3 MPa Grade Count:314
 9.00 - 140.653 MPa
@Temperature -40.0 - 120 °C
1310 - 20400.0 psi
@Temperature -40.0 - 248 °F
Average value: 58.0 MPa Grade Count:30
Tensile Strength, Yield 6.20 - 111 MPa899 - 16100 psiAverage value: 75.2 MPa Grade Count:223
Elongation at Break 0.900 - 98.0 %0.900 - 98.0 %Average value: 4.73 % Grade Count:335
 1.30 - 7.50 %
@Temperature -40.0 - 100 °C
1.30 - 7.50 %
@Temperature -40.0 - 212 °F
Average value: 3.08 % Grade Count:27
Elongation at Yield 2.00 - 9.40 %2.00 - 9.40 %Average value: 3.56 % Grade Count:78
 2.50 - 4.00 %
@Temperature 60.0 - 90.0 °C
2.50 - 4.00 %
@Temperature 140 - 194 °F
Average value: 3.25 % Grade Count:1
Modulus of Elasticity 2.25 - 15.0 GPa326 - 2180 ksiAverage value: 6.33 GPa Grade Count:225
 3.30 - 11.0 GPa
@Temperature -40.0 - 100 °C
479 - 1600 ksi
@Temperature -40.0 - 212 °F
Average value: 5.19 GPa Grade Count:27
Flexural Yield Strength 32.0 - 260 MPa4640 - 37700 psiAverage value: 118 MPa Grade Count:322
 70.0 - 234.422 MPa
@Temperature -40.0 - 121 °C
10200 - 34000.1 psi
@Temperature -40.0 - 250 °F
Average value: 112 MPa Grade Count:23
Flexural Modulus 0.115 - 8.85 GPa16.7 - 1280 ksiAverage value: 5.25 GPa Grade Count:504
 1.60 - 8.34266 GPa
@Temperature -40.0 - 121 °C
232 - 1210.02 ksi
@Temperature -40.0 - 250 °F
Average value: 4.91 GPa Grade Count:26
Compressive Yield Strength 57.9 - 82.7 MPa8400 - 12000 psiAverage value: 71.7 MPa Grade Count:7
Izod Impact, Notched 0.320 - 4.15 J/cm0.599 - 7.77 ft-lb/inAverage value: 1.12 J/cm Grade Count:254
 0.300 - 4.35 J/cm
@Temperature -40.0 - 121 °C
0.562 - 8.15 ft-lb/in
@Temperature -40.0 - 250 °F
Average value: 1.39 J/cm Grade Count:27
 0.5339 - 0.5339 J/cm
@Temperature -28.9 - -28.9 °C
1.000 - 1.000 ft-lb/in
@Temperature -20.0 - -20.0 °F
Average value: 1.39 J/cm Grade Count:1
 0.5339 - 0.5339 J/cm
@Thickness 3.17 - 3.17 mm
1.000 - 1.000 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 1.39 J/cm Grade Count:1
Izod Impact, Unnotched 0.650 - 8.54 J/cm1.22 - 16.0 ft-lb/inAverage value: 5.12 J/cm Grade Count:81
 0.450 - 1.10 J/cm
@Temperature 0.000 - 0.000 °C
0.843 - 2.06 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.788 J/cm Grade Count:4
Izod Impact, Notched (ISO) 4.50 - 55.0 kJ/m²2.14 - 26.2 ft-lb/in²Average value: 13.3 kJ/m² Grade Count:93
 4.41 - 50.0 kJ/m²
@Temperature -45.0 - -20.0 °C
2.10 - 23.8 ft-lb/in²
@Temperature -49.0 - -4.00 °F
Average value: 11.0 kJ/m² Grade Count:21
Izod Impact, Unnotched (ISO) 18.0 - 21000 kJ/m²8.57 - 9990 ft-lb/in²Average value: 41.9 kJ/m² Grade Count:13
 18.0 - 68.0 kJ/m²
@Temperature -30.0 - -30.0 °C
8.57 - 32.4 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 41.4 kJ/m² Grade Count:5
Charpy Impact Unnotched 0.500 - 2100 J/cm²2.38 - 9990 ft-lb/in²Average value: 4.85 J/cm² Grade Count:156
 0.400 - 8.70 J/cm²
@Temperature -45.0 - 0.000 °C
1.90 - 41.4 ft-lb/in²
@Temperature -49.0 - 32.0 °F
Average value: 4.40 J/cm² Grade Count:80
Charpy Impact, Notched 0.280 - 5.00 J/cm²1.33 - 23.8 ft-lb/in²Average value: 1.61 J/cm² Grade Count:225
 0.100 - 3.50 J/cm²
@Temperature -40.0 - 0.000 °C
0.476 - 16.7 ft-lb/in²
@Temperature -40.0 - 32.0 °F
Average value: 1.23 J/cm² Grade Count:126
Gardner Impact 0.300 - 23.0 J0.221 - 17.0 ft-lbAverage value: 2.05 J Grade Count:38
 2.71164 - 2.71164 J
@Temperature -5.56 - -5.56 °C
2.00000 - 2.00000 ft-lb
@Temperature 22.0 - 22.0 °F
Average value: 2.71 J Grade Count:1
Puncture Energy 21.0 - 21.0 J
@Temperature -30.0 - -30.0 °C
15.5 - 15.5 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 21.0 J Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1000 - 3.00e+16 ohm-cm1000 - 3.00e+16 ohm-cmAverage value: 3.44e+15 ohm-cm Grade Count:35
Surface Resistance 1e+05 - 1.60e+15 ohm1e+05 - 1.60e+15 ohmAverage value: 5.98e+14 ohm Grade Count:20
Dielectric Constant 2.50 - 3.302.50 - 3.30Average value: 2.77 Grade Count:20
Dielectric Strength 17.7 - 40.0 kV/mm450 - 1020 kV/inAverage value: 25.0 kV/mm Grade Count:22
Dissipation Factor 0.00100 - 0.003000.00100 - 0.00300Average value: 0.00158 Grade Count:12
Arc Resistance 85.0 - 125 sec85.0 - 125 secAverage value: 109 sec Grade Count:8
Comparative Tracking Index 575 - 650 V575 - 650 VAverage value: 612 V Grade Count:32
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.00 - 72.0 µm/m-°C1.67 - 40.0 µin/in-°FAverage value: 42.3 µm/m-°C Grade Count:38
Thermal Conductivity 0.270 - 0.331 W/m-K1.87 - 2.30 BTU-in/hr-ft²-°FAverage value: 0.319 W/m-K Grade Count:9
Melting Point 145 - 220 °C293 - 428 °FAverage value: 164 °C Grade Count:76
Maximum Service Temperature, Air 65.0 - 160 °C149 - 320 °FAverage value: 117 °C Grade Count:12
Hot Ball Pressure Test 125 - 145 °C257 - 293 °FAverage value: 129 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 99.0 - 165 °C210 - 329 °FAverage value: 153 °C Grade Count:242
Deflection Temperature at 1.8 MPa (264 psi) 63.9 - 220 °C147 - 428 °FAverage value: 143 °C Grade Count:407
Deflection Temperature at 8.0 MPa 117 - 134 °C243 - 273 °FAverage value: 122 °C Grade Count:21
Vicat Softening Point 85.0 - 166 °C185 - 331 °FAverage value: 137 °C Grade Count:192
UL RTI, Electrical 65.0 - 230 °C149 - 446 °FAverage value: 88.6 °C Grade Count:7
UL RTI, Mechanical with Impact 65.0 - 230 °C149 - 446 °FAverage value: 88.6 °C Grade Count:7
UL RTI, Mechanical without Impact 65.0 - 230 °C149 - 446 °FAverage value: 88.6 °C Grade Count:7
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:214
Flame Spread 9.00 - 100 mm/min0.354 - 3.94 in/minAverage value: 29.0 mm/min Grade Count:11
Oxygen Index 20.0 - 29.0 %20.0 - 29.0 %Average value: 22.1 % Grade Count:18
Glow Wire Test 550 - 960 °C1020 - 1760 °FAverage value: 765 °C Grade Count:50
 
Processing PropertiesMetricEnglishComments
Processing Temperature 30.0 - 270 °C86.0 - 518 °FAverage value: 170 °C Grade Count:68
Nozzle Temperature 188 - 270 °C370 - 518 °FAverage value: 231 °C Grade Count:64
Die Temperature 200 - 270 °C392 - 518 °FAverage value: 241 °C Grade Count:34
Melt Temperature 145 - 302 °C293 - 576 °FAverage value: 229 °C Grade Count:253
Mold Temperature 4.00 - 100 °C39.2 - 212 °FAverage value: 52.7 °C Grade Count:259
Injection Velocity 13.0 - 200 mm/sec0.512 - 7.87 in/secAverage value: 98.4 mm/sec Grade Count:11
Drying Temperature 48.9 - 220 °C120 - 428 °FAverage value: 86.1 °C Grade Count:205
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.128 % Grade Count:68
Injection Pressure 2.76 - 130 MPa400 - 18900 psiAverage value: 75.4 MPa Grade Count:127
Hot-Working Temperature 230 - 270 °C446 - 518 °FAverage value: 253 °C Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Overview of materials for Polypropylene with 40% Glass Fiber Filler
Overview of materials for Polypropylene with 60% Glass Fiber Filler

O4713 / 78378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.