MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Duplex
Categories: Metal; Ferrous Metal; Duplex

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Duplex". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.70 - 7.85 g/cc0.278 - 0.284 lb/in³Average value: 7.80 g/cc Grade Count:34
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 180 - 310180 - 310Average value: 256 Grade Count:18
Hardness, Rockwell C 15.0 - 32.015.0 - 32.0Average value: 27.8 Grade Count:16
Hardness, Vickers 250 - 900250 - 900Average value: 646 Grade Count:5
Tensile Strength, Ultimate 600 - 2730 MPa87000 - 396000 psiAverage value: 917 MPa Grade Count:42
Tensile Strength, Yield 400 - 2050 MPa58000 - 297000 psiAverage value: 610 MPa Grade Count:42
Elongation at Break 1.00 - 40.0 %1.00 - 40.0 %Average value: 23.6 % Grade Count:36
Modulus of Elasticity 190 - 205 GPa27500 - 29700 ksiAverage value: 199 GPa Grade Count:29
Poissons Ratio 0.250 - 0.3330.250 - 0.333Average value: 0.305 Grade Count:14
Fatigue Strength 446 - 802 MPa64700 - 116000 psiAverage value: 579 MPa Grade Count:4
Shear Modulus 74.0 - 86.0 GPa10700 - 12500 ksiAverage value: 77.2 GPa Grade Count:14
Charpy Impact 90.0 - 150 J66.4 - 111 ft-lbAverage value: 114 J Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000800 - 0.0000850 ohm-cm0.0000800 - 0.0000850 ohm-cmAverage value: 0.0000814 ohm-cm Grade Count:11
Magnetic Permeability 25.0 - 12025.0 - 120Average value: 77.0 Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 - 14.5 µm/m-°C6.67 - 8.06 µin/in-°FAverage value: 13.3 µm/m-°C Grade Count:8
Specific Heat Capacity 0.418 - 0.590 J/g-°C0.100 - 0.141 BTU/lb-°FAverage value: 0.481 J/g-°C Grade Count:30
Thermal Conductivity 13.0 - 17.0 W/m-K90.2 - 118 BTU-in/hr-ft²-°FAverage value: 15.0 W/m-K Grade Count:27
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 950 - 1120 °C1740 - 2050 °FAverage value: 1050 °C Grade Count:4
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.0200 - 0.0800 %0.0200 - 0.0800 %Average value: 0.0301 % Grade Count:40
Chromium, Cr 18.5 - 27.5 %18.5 - 27.5 %Average value: 23.2 % Grade Count:41
Copper, Cu 0.0500 - 3.30 %0.0500 - 3.30 %Average value: 1.16 % Grade Count:12
Iron, Fe 55.2 - 72.7 %55.2 - 72.7 %Average value: 66.0 % Grade Count:41
Manganese, Mn 0.500 - 5.00 %0.500 - 5.00 %Average value: 1.78 % Grade Count:31
Molybdenum, Mo 0.0500 - 5.00 %0.0500 - 5.00 %Average value: 2.80 % Grade Count:40
Nickel, Ni 1.50 - 11.0 %1.50 - 11.0 %Average value: 5.68 % Grade Count:41
Nitrogen, N 0.0500 - 0.320 %0.0500 - 0.320 %Average value: 0.186 % Grade Count:35
Phosphorus, P 0.0250 - 0.0400 %0.0250 - 0.0400 %Average value: 0.0315 % Grade Count:20
Silicon, Si 0.400 - 1.60 %0.400 - 1.60 %Average value: 0.955 % Grade Count:30
Sulfur, S 0.00100 - 0.0300 %0.00100 - 0.0300 %Average value: 0.0147 % Grade Count:22

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Carbon Steel
Overview of materials for Medium Carbon Steel
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
ASTM A542 Low Alloy Steel, Grade A, Class 4
AK Steel 304 Austenitic Stainless steel

M01016 / 81718

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.