MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® B40 Nylon PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Vydyne B40 is high viscosity PA6 for extrusion applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 2.35 %2.35 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 10 %10 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psiDAM; ISO 527-2
Elongation at Break 15 %15 %DAM; ISO 527-2
Elongation at Yield 4.0 %4.0 %DAM; ISO 527-2
Tensile Modulus 3.10 GPa450 ksiDAM; ISO 527-2
Flexural Strength 100 MPa14500 psiDAM; ISO 178
Flexural Modulus 2.70 GPa392 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  3.00 kJ/m²
@Temperature -40.0 °C
1.43 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO)  100 kJ/m²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1U
 100 kJ/m²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical  65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 240 °C446 - 464 °FInjection
Middle Barrel Temperature 240 - 250 °C464 - 482 °FInjection
Front Barrel Temperature 250 - 260 °C482 - 500 °FInjection
Melt Temperature 250 - 260 °C482 - 500 °FInjection
Mold Temperature 60.0 - 80.0 °C140 - 176 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
Moisture Content 0.20 %0.20 %Injection
 
Descriptive Properties
AdditiveRelease agent
Agency RatingsISO, 1043 PA6
AppearanceNatural Color
FormsPellets
Processing MethodOther Extrusion
 Profile Extrusion
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8824 / 293393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.