MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem SGF4950TT Biobased Copolymer high-density polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: SGF4950TT is a copolymer high-density polyethylene without optical brightener in it composition, developed for the blow-molding segment with well-balanced properties between impact and stiffness, combined with high environmental stress cracking resistance and processability. The minimum biobased carbon content of this grade is 96%, determined according to ASTM D6866.
Applications: Tissue and hygiene packaging, Polymer blends, Cosmetic packaging.
Process: Blow molding.

Test specimens from compression molded plaque according to ASTM D4703. Plaque Thickness 2mm.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc0.0345 lb/in³ASTM D792
ESCR 10% Igepal® 30 hour
@Thickness 0.300 mm,
Temperature 50.0 °C
30 hour
@Thickness 0.0118 in,
Temperature 122 °F
Notched. CO630.; ASTM D1693
Melt Flow  0.34 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.34 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 28 g/10 min
@Load 21.6 kg,
Temperature 190 °C
28 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 MPa4350 psiASTM D638
Tensile Strength, Yield 30.0 MPa4350 psiASTM D638
Flexural Modulus, 1% Secant 1250 MPa181000 psiASTM D790
Tensile Impact Strength 110 kJ/m²52.3 ft-lb/in²ISO 8256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648
Vicat Softening Point 127 °C
@Load 1.02 kg
261 °F
@Load 2.25 lb
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS604 / 313997

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.