MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Categories: Ceramic; Oxide; Wood and Natural Products

Material Notes: Calcium hydroxyapatite is a natural constituent of teeth and bone, along with other calcium-phosphate ceramic (CPC) materials. Synthetic hydroxyapatite is used as an active bioceramic for teeth and bone replacement. Ionic substitution is common and plays a large role in the structure and properties of hydroxyapatites.

Key Words: Ca10(PO4)6(OH)2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.05 - 3.15 g/cc0.110 - 0.114 lb/in³
 3.219 g/cc0.1163 lb/in³Calculated (for zero porosity)
Porosity 0.10 - 3.0 %0.10 - 3.0 %
a Lattice Constant 9.432 Å9.432 Å
c Lattice Constant 6.881 Å6.881 Å
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 38.0 - 48.0 MPa5510 - 6960 psi
Modulus of Elasticity 7.00 - 13.0 GPa1020 - 1890 ksi
Flexural Strength 100 - 120 MPa14500 - 17400 psi
Compressive Strength 350 - 450 MPa50800 - 65300 psi
Poissons Ratio 0.270.27
Shear Modulus 2.76 - 5.12 GPa400 - 743 ksiCalculated
 
Descriptive Properties
Unit CellHexagonal

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
Titanium, Ti
Silicon Nitride
Thoracic aorta Human Artery
Overview of materials for Low Density Polyethylene (LDPE), Molded

BBIOC00 / 149

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.