MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemical Concepts PERMATEX® #26 High-Temp RTV Silicone Gasket
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Permatex® High-Temp RTV Silicone Gasket is a single component, room temperature vulcanizing gasketing compound designed to provide reliable “formed-in-place” gaskets for mechanical assemblies. This material cures on exposure to moisture in the air to form a tough, flexible, silicone rubber gasket. The product resists aging, weathering and thermal cycling without hardening, shrinking or cracking. Designed to maintain maximum performance in a continuous temperature environment of 600°F. Conforms to MIL-A46106B, Type I. Certified to NSF/ANSI Standard 51.

Features:

  • High temperature use
  • Superior adhesion and flexibility
  • Replaces most cut gaskets
  • Can be used as a gasket maker or dressing
  • Easy application
  • Non-flammable
  • Non-toxic
Uses:
  • Sealing panels
  • Window plates
  • Oven doors
  • Flues on high temperature applications.
    • Permatex® High-Temp RTV Silicone Gasket cures on exposure to moisture in air. The product dries tack free in one hour and fully cures in 24 hours. Cure times will vary with temperature, humidity and gap. The curing process can cause corrosion to some surfaces, for critical applications use the Ultra Series silicones. The product retains effective properties in contact with automotive fluids, such as motor oil, transmission fluids, alcohol and antifreeze solutions. Not recommended for parts in contact with gasoline. This product is not recommended for use in pure oxygen and/or oxygen rich systems and should not be selected as a sealant for chlorine or other strong oxidizing materials.

      Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
 1.05 g/cc1.05 g/ccuncured material
Volatile Organic Compounds (VOC) Content 30 g/l30 g/l
Vapor Pressure 0.0133 bar
@Temperature 26.7 °C
10.0 torr
@Temperature 80.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 20
@Temperature 25.0 °C
>= 20
@Temperature 77.0 °F
After 7 days of curing. 50% RH.
Tensile Strength at Break >= 1.50 MPa>= 218 psiAfter 7 days of curing. 50% RH.
Elongation at Break >= 350 %>= 350 %After 7 days of curing. 50% RH.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 316 °C600 °Fcontinuous
Flash Point >= 93.0 °C>= 199 °Funcured material
 >= 93.3 °C>= 200 °FTag closed cup
 
Processing PropertiesMetricEnglishComments
Extrusion Rate >= 220 g/min
@Temperature 25.0 °C
>= 220 g/min
@Temperature 77.0 °F
uncured material
 
Component Elements PropertiesMetricEnglishComments
TiO2 1.0 - 10 %1.0 - 10 %by weight
 
Descriptive Properties
Amorphous Silica (%)5-15, by weight
AppearanceRed non-sag paste. Uncured material.
Dimethyl Siloxane, hydroxy-terminated (%)>60 by weight
Distillates (petroleum), hydrotreated middle (%)1-10, by weight
Ethyltriacetoxysilane (%)1-10, by weight
Gap Fill (in)0.25. After 7 days of curing at 25°C, 50% RH.
Iron Oxide (%)1-10, by weight
Methyltriacetoxysilane (%)1-10, by weight
OdorMild acetic. Uncured material.
Polydimethyl Siloxane (%)1-10, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black
Henkel Loctite® Nuva-Sil® 5091 High Adhesion Potting

PCHEMI981 / 232152

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.