MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Martensitic Nickel-Chromium Iron, abrasion resistant
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron

Material Notes: Martensite, austenite matrix structure as cast. Cu content may replace all or part of the Ni.

Key Words: Abrasion resistant martensitic nickel-chromium iron, martensitic, austenitic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.61 - 7.81 g/cc0.275 - 0.282 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000800 ohm-cm0.0000800 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 - 9.00 µm/m-°C
@Temperature 10.0 - 260 °C
4.44 - 5.00 µin/in-°F
@Temperature 50.0 - 500 °F
Thermal Conductivity 30.0 W/m-K208 BTU-in/hr-ft²-°FEstimated.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.5 - 3.7 %2.5 - 3.7 %
Chromium, Cr 1.1 - 4.0 %1.1 - 4.0 %
Iron, Fe 87 %87 %
Manganese, Mn <= 1.3 %<= 1.3 %
Molybdenum, Mo <= 1.0 %<= 1.0 %
Nickel, Ni 2.7 - 5.0 %2.7 - 5.0 %
Phosphorus, P <= 0.30 %<= 0.30 %
Silicon, Si <= 0.80 %<= 0.80 %
Sulfur, S <= 0.15 %<= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Alloy Cast Iron
High-Nickel Gray Iron, corrosion resistant
High-Chromium Iron, corrosion resistant
Low-C White Iron, abrasion resistant
High-Nickel Ductile Iron, corrosion resistant

MAFEA2 / 10232

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.