MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Hyflon® PFA M640 Perfluoroalkoxy (PFA)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, inherent flame resistance, low surface energy, and exceptional dielectric properties. Hyflon® PFA resins have been designed to retain their properties over a wide range of temperatures from cryogenic to 250-260°C (482-500°F) and are the material of choice in applications such as linings in the Chemical Process Industry, specialty cables, semiconductor industry, aerospace, and other challenging industries.

Hyflon® PFA M640 is a high melt flow rate multi-purpose resin designed for pipe, cable, and stock shapes extrusion, injection, compression, and transfer molding. Hyflon® PFA M640 has obtained UL758 recognition for continuous use at 250°C (482°F) and is an ASTM D3307 - Type VII resin.

Applications: Aerospace Applications; Cable Jacketing; Liners; Piping; Semiconductor Molding Compounds

Features: Flame Retardant; High Heat Resistance; Low Flow; Semi Crystalline

PROCESSING
- Because PFA is corrosive in the melt, machinery used to process Hyflon® should be lined with corrosion resistant alloys. Clean, reworked material can be used up to 25% in weight.

HEALTH SAFETY AND ENVIRONMENT
- Hyflon® PFA M640 is a very inert polymer and it is not harmful if used and handled according to standard processing procedures. If handled inappropriately, it may release harmful toxic chemicals.

PACKAGING AND STORAGE
- Hyflon® PFA M640 resin is available in 25 kg (55 lbs.) and 500 kg (1102 lbs.) packaging. Though it has an indefinite shelf life, it is recommended to store it in a clean area, protected from direct sunlight and possible contamination.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.13 - 2.18 g/cc0.0770 - 0.0788 lb/in³ASTM D792
Melt Flow 10 - 17 g/10 min
@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min
@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 6055 - 60ASTM D2240
Tensile Strength at Break >= 21.0 MPa>= 3050 psiASTM D638
Elongation at Break >= 280 %>= 280 %ASTM D638
Tensile Modulus 0.500 - 0.600 GPa72.5 - 87.0 ksi1.0 mm/min; ASTM D638
Izod Impact, Notched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D257
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant  2.0
@Frequency 50 Hz
2.0
@Frequency 50 Hz
ASTM D150
 2.0
@Frequency 100000 Hz
2.0
@Frequency 100000 Hz
ASTM D150
Dielectric Strength 35.0 - 40.0 kV/mm889 - 1020 kV/inASTM D149
Dissipation Factor  <= 0.00050
@Frequency 50 Hz
<= 0.00050
@Frequency 50 Hz
ASTM D150
 <= 0.00050
@Frequency 100000 Hz
<= 0.00050
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 18.0 - 26.0 J/g7.74 - 11.2 BTU/lbDSC
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C66.7 - 111 µin/in-°FASTM D696
Specific Heat Capacity 0.900 - 1.10 J/g-°C0.215 - 0.263 BTU/lb-°FASTM C351
Thermal Conductivity 0.200 W/m-K
@Temperature 40.0 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 104 °F
ASTM C177
Melting Point 280 - 290 °C536 - 554 °F
Crystallization Temperature 255 - 265 °C491 - 509 °FPeak; ASTM D3418
Maximum Service Temperature, Air 250 °C482 °FContinuous; ASTM D794
Flammability, UL94 V-0V-0
Oxygen Index 95 %95 %ASTM D2863
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingCompression Molding; Extrusion; Injection Molding; Resin Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4250 / 280050

http://www.madehow.com/Volume-1/Tire.html

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.