MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Poly Alloy Etoma™ ET2202 PS with Carbon Black
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Carbon Black Filled

Material Notes: Etoma ET2202 resin is a conductive compound base on polystyrene with carbon black, designed to wide range application of anti-static package. With excellent mechanical properties, ET2202 can be used on application of carrier tapes with deep-drawing shapes. ET2202 has excellent elongation and appropriate melt flow rate, it can be processed with rapid linear velocity. This resin also has good heat resistance and stable electrical conductivity.

Information provided by Poly Alloy Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Melt Flow 1.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.8 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 25.5 MPa3700 psiASTM D638
Elongation at Break 18 %18 %ASTM D638
Flexural Strength 48.1 MPa6970 psiASTM D790
Flexural Modulus 2.21 GPa320 ksiASTM D790
Izod Impact, Notched 1.96 J/cm3.67 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 10000 - 1.00e+6 ohm10000 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C187 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 - 200 °C374 - 392 °F
Middle Barrel Temperature 210 - 220 °C410 - 428 °F
Front Barrel Temperature 200 - 210 °C392 - 410 °F
Nozzle Temperature 200 - 210 °C392 - 410 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 120 °C248 °F
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hour
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPALLOY029 / 278308

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.