MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Diofan® A 586 PVDC
Categories: Polymer; Thermoplastic; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC)

Material Notes: Diofan® A 586 is a PVDC aqueous dispersion specially designed for flexible to coats on cellulosic and textile casings.

Applications: Barrier Coatings; Coating Applications; Fabric Coatings; Non-wovens Coatings; Wovens Coatings

Features: Flame Retardant; Low VOC; Moisture Barrier; Non-Toxic; Oxygen BarrierDiofan® A 586 is delivered in bulk or in Intermediate Bulk Containers (IBC). Bulk supplied latex should be stored in reservoirs made of suitable stainless steel, HDPE, rigid PVC or glass fiber-reinforced polyester.
- Contact of anionic Diofan® dispersion with metals like iron, zinc, aluminum and copper as well as alloys such as brass and bronze must be avoided.
- Keep the vessels tightly closed to prevent drying through evaporation. Store the product ideally between 5°C and 30°C (41 °F and 86°F) to avoid degradation.

PROCESSING - DRYING
- Diofan® A 586 can be processed with different coating techniques, including reverse gravure roll and air knife coating systems.
- When coated on plastic films, Diofan® A 586 should be formulated with wax and silica in order to improve the blocking and slip properties of the finished coating.
- Diofan® coatings requires adequate drying conditions, since in general higher temperatures will contribute to better barrier properties.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³
pH 1.51.5
Viscosity 14 cP
@Temperature 20.0 °C
14 cP
@Temperature 68.0 °F
 
Descriptive Properties
AvailabilityEurope
ColorMilky White
FormsLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4168 / 279968

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.