System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
ICO Polymers ICOTEX™ 520-5059 500 Micron LDPE Powder
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Low Density (LDPE)
;
Low Density Polyethylene (LDPE), Masterbatch Grade
Material Notes:
Description:
ICOTEX 520-5059 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry.
Information provided by ICO Polymers.
A Schulman acquired ICO, Inc. in 2010.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.915
g/cc
0.0331
lb/in³
ASTM D1505
Particle Size
>=
150
µm
>=
150
µm
pan, 13%
<=
500
µm
<=
500
µm
sieve < 5%
Melt Index of Compound
8.0
g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties
Metric
English
Comments
Melting Point
104
°C
219
°F
DSC; ASTM D3418
Vicat Softening Point
86.0
°C
187
°F
ASTM D1525
Descriptive Properties
Max Dry Flow
max 31 sec/100g
ASTM
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PICO039 / 48012
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.