MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Toyobo Zenite® 251 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Unfilled

Material Notes: Product Description: This LCP is designed for low dielectric constant (Dk), excellent flow characteristics & mechanical strength and high temperature resistance. For use in injection molded electronics applications for thin walls.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Maximum Moisture Content 0.0100.010
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiISO 527-2/5
Elongation at Break 1.9 %1.9 %ISO 527-2/5
Tensile Modulus 7.38 GPa1070 ksiISO 527-1
Flexural Strength 139 MPa20200 psiISO 178
Flexural Modulus 7.03 GPa1020 ksiISO 178
Charpy Impact Unnotched 0.630 J/cm²3.00 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0029
@Frequency 100 Hz
0.0029
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance >= 127 sec>= 127 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.9 µm/m-°C8.30 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 50.4 µm/m-°C28.0 µin/in-°FISO 11359-2
Melting Point 350 °C662 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FUnannealed; ISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.406 mm
V-0
@Thickness 0.0160 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 340 - 350 °C644 - 662 °F
Middle Barrel Temperature 350 - 360 °C662 - 680 °F
Front Barrel Temperature 360 - 370 °C680 - 698 °F
Nozzle Temperature 370 - 380 °C698 - 716 °F
Zone 4 370 - 380 °C698 - 716 °FInjection
Mold Temperature 100 °C212 °F
Drying Temperature 150 °C302 °F
Dry Time 4.00 hour4.00 hour
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Back Pressure <= 3.00 MPa<= 435 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6325 / 311018

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.