MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SCb-291 Niobium Alloy
Categories: Metal; Nonferrous Metal; Niobium Alloy; Refractory Metal

Material Notes: Nb-10Ta-10W

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 10.5 g/cc0.379 lb/in³estimated by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 221 MPa
@Temperature 1090 °C
32000 psi
@Temperature 2000 °F
Recrystallized
Rupture Strength 62.1 MPa
@Temperature 1090 °C,
Time 36000 sec
9000 psi
@Temperature 2000 °F,
Time 10.0 hour
Recrystallized
 
Component Elements PropertiesMetricEnglishComments
Niobium, Nb (Columbium, Cb) 80 %80 %As balance
Tantalum, Ta 10 %10 %
Tungsten, W 10 %10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Niobium C-103 (WC 103; 89Nb-10Hf-1Ti), Cold-Rolled
WC-3009 Niobium Alloy
Elmet-Starck Pure Niobium (Columbium)
H.C. Starck Amperit® 161.065 Niobium (Nb)
H.C. Starck Grain Stabilized Niobium (GSNb)

MRNb56 / 100349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.