MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless; Tool Steel; Mold Steel

Material Notes: A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-supplied hardness of 34-36 HRC, or a low-temperature aging treatment can increase the hardness up to 50 HRC.

CORRAX® is characterized by:

  • Extremely good dimensional stability during the aging process
  • High uniformity of properties even in large dimensions
  • Very good weldability; no pre-heating necessary
  • No hard "white layer" after EDM
  • Corrosion resistance superior to AISI 420 and AISI 440C

Applications:

  • Injection moulds for corrosive plastics, rubber and medical and food industry
  • Extrusion dies
  • Plastic processing - screws
  • Engineering parts

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.75 g/cc0.280 lb/in³hardened to 46 HRC
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell C 3434Solution treated (Delivery condition)
    Tensile Strength, Ultimate 1100 MPa160000 psiSolution treated ~ 34 HRC
     1170 MPa170000 psiAged to ~ 40 HRC
     1520 MPa220000 psiAged to ~ 46 HRC
     1720 MPa250000 psiAged to ~ 50 HRC
    Tensile Strength, Yield 1590 MPa230000 psiAged to ~ 50 HRC
     689 MPa
    @Strain 0.2 %
    100000 psi
    @Strain 0.2 %
    Solution treated ~ 34 HRC
     1030 MPa
    @Strain 0.2 %
    150000 psi
    @Strain 0.2 %
    Aged to ~ 40 HRC
     1380 MPa
    @Strain 0.2 %
    200000 psi
    @Strain 0.2 %
    Aged to ~ 46 HRC
    Modulus of Elasticity 200 GPa29000 ksi(hardened to 46 HRC)
     172 GPa
    @Temperature 399 °C
    25000 ksi
    @Temperature 750 °F
    hardened to 46 HRC
     193 GPa
    @Temperature 199 °C
    28000 ksi
    @Temperature 390 °F
    hardened to 46 HRC
    Compressive Yield Strength 900 MPa131000 psi0.2%, Solution treated ~ 34 HRC
     1300 MPa189000 psi0.2%, Aged to ~ 40 HRC
     1600 MPa232000 psi0.2%, Aged to ~ 46 HRC
     1800 MPa261000 psi0.2%, Aged to ~ 50 HRC
    Impact Test 5.42 - 17.6 J4.00 - 13.0 ft-lb50 HRC
     20.3 - 40.7 J15.0 - 30.0 ft-lb34 HRC
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  11.7 µm/m-°C
    @Temperature 199 °C
    6.50 µin/in-°F
    @Temperature 390 °F
    hardened to 46 HRC
     12.2 µm/m-°C
    @Temperature 399 °C
    6.80 µin/in-°F
    @Temperature 750 °F
    hardened to 46 HRC
    Thermal Conductivity  18.0 W/m-K
    @Temperature 199 °C
    125 BTU-in/hr-ft²-°F
    @Temperature 390 °F
    hardened to 46 HRC
     21.0 W/m-K
    @Temperature 399 °C
    146 BTU-in/hr-ft²-°F
    @Temperature 750 °F
    hardened to 46 HRC
    Shrinkage  0.070 - 0.25 %
    @Temperature 524 - 621 °C,
    Time 14400 sec
    0.070 - 0.25 %
    @Temperature 975 - 1150 °F,
    Time 4.00 hour
     0.070 - 0.25 %
    @Temperature 524 - 621 °C,
    Time 14400 sec
    0.070 - 0.25 %
    @Temperature 975 - 1150 °F,
    Time 4.00 hour
    Transverse
     
    Component Elements PropertiesMetricEnglishComments
    Aluminum, Al 1.6 %1.6 %
    Carbon, C 0.030 %0.030 %
    Chromium, Cr 12 %12 %
    Iron, Fe 75.17 %75.17 %as balance
    Manganese, Mn 0.30 %0.30 %
    Molybdenum, Mo 1.4 %1.4 %
    Nickel, Ni 9.2 %9.2 %
    Silicon, Si 0.30 %0.30 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Bohler-Uddeholm UDDEHOLM RAMAX® LH Plastic Mold Steel
    Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
    Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
    Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel
    Bohler-Uddeholm M238 VMR® P20 Plastic Lens Mold Steel

    NBUCOR23 / 15492

    New MatWeb Services

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.