MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Description

Polyfort® PP 3153 is a homopolymer polypropylene.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 - 0.910 g/cc0.890 - 0.910 g/ccASTM D792
Melt Flow 4.5 - 7.5 g/10 min
@Temperature 230 °C
4.5 - 7.5 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8080ASTM D785
Tensile Strength, Yield 26.5 MPa3840 psiASTM D638
Elongation at Break 300 %300 %ASTM D638
Flexural Strength 29.0 MPa4210 psiASTM D790
Flexural Modulus 0.931 GPa135 ksiASTM D790
Izod Impact, Notched 0.801 J/cm1.50 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Americas Styrenics MC3650 High Heat Crystal Polystyrene
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene
A. Schulman PP 3479-01 Polypropylene Random Copolymer
A. Schulman PP 1632-01 Polypropylene Random Copolymer

PASHU198 / 25162

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.