MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Epoxy, Thermally Conductive
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Thermally Conductive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.670 - 4.45 g/cc0.0242 - 0.161 lb/in³Average value: 1.82 g/cc Grade Count:96
Water Absorption 0.100 - 0.500 %0.100 - 0.500 %Average value: 0.172 % Grade Count:9
Particle Size 20.0 - 500 µm20.0 - 500 µmAverage value: 56.3 µm Grade Count:48
Viscosity 10.0 - 819000 cP10.0 - 819000 cPAverage value: 82600 cP Grade Count:115
 800 - 120000 cP
@Temperature 40.0 - 100 °C
800 - 120000 cP
@Temperature 104 - 212 °F
Average value: 13500 cP Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 15.0 - 85.015.0 - 85.0Average value: 53.2 Grade Count:6
Hardness, Shore D 15.0 - 10015.0 - 100Average value: 82.6 Grade Count:112
 24.0 - 28.0
@Temperature 100 - 149 °C
24.0 - 28.0
@Temperature 212 - 300 °F
Average value: 52.4 Grade Count:4
Tensile Strength, Ultimate 0.820 - 552 MPa119 - 80000 psiAverage value: 45.1 MPa Grade Count:43
Elongation at Break 0.200 - 70.0 %0.200 - 70.0 %Average value: 16.4 % Grade Count:13
Modulus of Elasticity 0.0179 - 20.0 GPa2.60 - 2900 ksiAverage value: 5.48 GPa Grade Count:81
 2.362 - 4.25 GPa
@Temperature 0.000 - 100 °C
342.6 - 616 ksi
@Temperature 32.0 - 212 °F
Average value: 3.31 GPa Grade Count:1
Flexural Yield Strength 180 - 579 MPa26100 - 84000 psiAverage value: 404 MPa Grade Count:4
Compressive Yield Strength 68.9 - 207 MPa10000 - 30000 psiAverage value: 151 MPa Grade Count:22
Shear Strength 3.20 - 53.8 MPa464 - 7800 psiAverage value: 20.0 MPa Grade Count:50
Adhesive Bond Strength 1.72 - 27.6 MPa250 - 4000 psiAverage value: 11.8 MPa Grade Count:47
Izod Impact, Notched 0.160 - 53.4 J/cm0.300 - 100 ft-lb/inAverage value: 17.9 J/cm Grade Count:3
Peel Strength 0.789 - 10.5 kN/m4.50 - 60.0 pliAverage value: 2.51 kN/m Grade Count:15
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00100 - 1.00e+16 ohm-cm0.00100 - 1.00e+16 ohm-cmAverage value: 6.27e+14 ohm-cm Grade Count:103
 2.00e+13 - 3.20e+13 ohm-cm
@Temperature 75.0 - 75.0 °C
2.00e+13 - 3.20e+13 ohm-cm
@Temperature 167 - 167 °F
Average value: 2.90e+13 ohm-cm Grade Count:4
Surface Resistance 1.50e+12 - 4.40e+14 ohm1.50e+12 - 4.40e+14 ohmAverage value: 8.57e+13 ohm Grade Count:5
Dielectric Constant 3.12 - 7.803.12 - 7.80Average value: 4.81 Grade Count:95
Dielectric Strength 7.40 - 78.7 kV/mm188 - 2000 kV/inAverage value: 21.4 kV/mm Grade Count:41
Dissipation Factor 0.00100 - 0.1460.00100 - 0.146Average value: 0.0120 Grade Count:60
Arc Resistance 120 - 193 sec120 - 193 secAverage value: 154 sec Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.4 - 239 µm/m-°C5.78 - 133 µin/in-°FAverage value: 61.0 µm/m-°C Grade Count:100
CTE, linear, Transverse to Flow 22.0 - 246 µm/m-°C12.2 - 137 µin/in-°FAverage value: 101 µm/m-°C Grade Count:6
 175 - 192 µm/m-°C
@Temperature >=160 °C
97.2 - 107 µin/in-°F
@Temperature >=320 °F
Average value: 184 µm/m-°C Grade Count:2
Thermal Conductivity 0.100 - 17.0 W/m-K0.694 - 118 BTU-in/hr-ft²-°FAverage value: 1.54 W/m-K Grade Count:120
 0.800 - 1.50 W/m-K
@Temperature 80.0 - 121 °C
5.55 - 10.4 BTU-in/hr-ft²-°F
@Temperature 176 - 250 °F
Average value: 1.15 W/m-K Grade Count:2
Maximum Service Temperature, Air 100 - 375 °C212 - 707 °FAverage value: 220 °C Grade Count:121
Minimum Service Temperature, Air -269 - -20.0 °C-453 - -4.00 °FAverage value: -66.0 °C Grade Count:116
Glass Transition Temp, Tg -27.0 - 215 °C-16.6 - 419 °FAverage value: 91.3 °C Grade Count:79
Decomposition Temperature 291 - 486 °C556 - 907 °FAverage value: 386 °C Grade Count:53
Flammability, UL94 V-0V-0Grade Count:6
 
Processing PropertiesMetricEnglishComments
Cure Time 8.00 - 10100 min0.133 - 168 hourAverage value: 2280 min Grade Count:53
 1.00 - 1440 min
@Temperature 45.0 - 204 °C
0.0167 - 24.0 hour
@Temperature 113 - 400 °F
Average value: 118 min Grade Count:116
Pot Life 5.00 - 130000 min5.00 - 130000 minAverage value: 7560 min Grade Count:95
 30.0 - 30.0 min
@Temperature 60.0 - 80.0 °C
30.0 - 30.0 min
@Temperature 140 - 176 °F
Average value: 105 min Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Electrically Conductive
Overview of materials for Epoxy, High Temperature
Overview of materials for Epoxy Molding Compound
Overview of materials for Epoxy, Cast, Unreinforced
Overview of materials for Epoxy Cure Resin

O1726 / 120755

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.