MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Diamond, Natural
Categories: Carbon; Diamond; Pure Element

Key Words: Diamonds, Carbon, C
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 3.51 - 3.52 g/cc0.127 - 0.127 lb/in³
a Lattice Constant 3.5597 Å3.5597 Å
Volume Compressibility, 10^-10 m²/N 1818
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 12.010712.01071995
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 80008000
Knoop Microhardness 58 - 8858 - 88GPa; (110),(111) faces
 7979GPa
 56 - 10256 - 102GPa; (001) face
Vickers Microhardness 9898in GPa; (111) face
 88 - 14788 - 147in GPa; (001) face
Hardness, Mohs 1010
Abrasive Hardness 140000140000
Modulus of Elasticity 700 - 1200 GPa102000 - 174000 ksi
Compressive Strength 8680 - 16530 MPa1.26e+6 - 2.397e+6 psi
Poissons Ratio 0.10 - 0.290.10 - 0.29
Fracture Toughness 3.40 MPa-m½3.09 ksi-in½
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.00000588-0.00000588Atomic (cgs)
Dielectric Constant 5.5 - 5.7
@Frequency 1e+6 Hz
5.5 - 5.7
@Frequency 1e+6 Hz
Dielectric Strength 1000 kV/mm25400 kV/in
Dissipation Factor 0.000200.00020
Band Gap 5.2 - 5.6 eV
@Temperature 0.000 °C
5.2 - 5.6 eV
@Temperature 32.0 °F
Electron Mobility, cm²/V-s 1800 - 22001800 - 2200
Hole Mobility, cm²/V-s 1200 - 16001200 - 1600
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.18 µm/m-°C
@Temperature 20.0 °C
0.656 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.5079 J/g-°C0.1214 BTU/lb-°FCrystal
Thermal Conductivity 2000 W/m-K13900 BTU-in/hr-ft²-°F
Heat of Formation 1.900 kJ/mol1.900 kJ/molCrystal
Debye Temperature 2067 °C3753 °F
Decomposition Temperature 707 °C1300 °FTransition to graphite
 
Optical PropertiesMetricEnglishComments
Refractive Index 2.4192.419
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 100 %100 %
 
Descriptive Properties
CAS Number7782-40-3
ColorClearImpurities (i.e. Nitrogen) and irradiation can change color to yellow, green, blue, pink, or brown.
Crystal StructureCubicDiamond - Space Group Fd3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Diamond, Synthetic
Diamond, Polycrystalline
Graphite, Carbon, C
Diamond, thin film
BACT DLC Diamond-Like Coating

CDiamA / 771

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.