MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubriplate HP-2 Poly Polyurea-Thickened Type Grease For Special Applications / Conditions
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Polyurea-thickened type grease formulated with the highest quality paraffinic base oils available. Excellent for high speed electric motor bearings and other industrial applications.

Applications: Electric motor bearings.

Poly HP-2 is available in Cartridges, Pails & 1/4 Drums.

Information provided by Lubriplate

Key Words: Part Number L0191-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Saybolt Viscosity at 100°F 650 SUS650 SUS
Kinematic Viscosity at 40°C (104°F) 128 cSt128 cSt
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 265265Unknown Amount of Work
Penetration P(60), 1/10 mm 295295Unknown Amount of Work
 
Thermal PropertiesMetricEnglishComments
Dropping Point 260 °C500 °FASTM Test
 
Descriptive Properties
Antiwear (AW)/ Extreme Pressure (EP)AW
NLGI Grade2
Rust/Oxidative AdditivesYES
Water ResistantYES

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron L060330-2 Flexible Polyurea Compound
Phillips 66 Polyurea NLGI Grade No. 1
CHT Group EP RP EPI Engineered Polymers Aromatic Polyurea
CHT Group EP RAP 45 EPI Engineered Polymers Aliphatic Polyurea

WLUBR079 / 76125

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.