MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 699 X 113386 B Acrylonitrile Butadiene Styrene (ABS) LDS Platable
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Plating Grade

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D 792
Linear Mold Shrinkage 0.0070 cm/cm
@Thickness 3.20 mm
0.0070 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 34.5 MPa5000 psiASTM D 638
Elongation at Break 6.0 - 10 %6.0 - 10 %ASTM D 638
Tensile Modulus 2.41 GPa350 ksiASTM D 638
Flexural Strength 62.1 MPa9000 psiASTM D 790
Flexural Modulus 2.28 GPa330 ksiASTM D 790
Izod Impact, Notched 1.33 J/cm
@Thickness 3.20 mm
2.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 13.3 J/cm
@Thickness 3.20 mm
25.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dissipation Factor 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 67.0 µm/m-°C37.2 µin/in-°FE 831
CTE, linear, Transverse to Flow 99.5 µm/m-°C55.3 µin/in-°FE 831
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C205 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 238 °C400 - 460 °F
Mold Temperature 62.8 - 85.0 °C145 - 185 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bhansali Engineering Abstron AP-78 EP ABS Electro Plating Applications
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
Ineos ABS Lustran® Ultra 4000 PG ABS Pellets (a-methylstyrene-SAN-modified), Electroplating Grade
Zeon Specialty Materials ZEONEX® RS420-LDS Cyclo Olefin Polymer
Lotte Advanced Materials Starex® MP-0670 ABS, Metal Plating Grade

PQZVA10584 / 120618

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.