MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Vestyron® 554 S Impact-Modified Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: Uses: Housings, cases and peripherals for electronics, printer housings.

ISO data as provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³
Water Absorption 0.00 %0.00 %
Melt Flow 11 g/10 min11 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 29.0 MPa4210 psi
Elongation at Break 30 %30 %
Elongation at Yield 1.0 %1.0 %
Modulus of Elasticity 2.60 GPa377 ksi
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  2.0
@Frequency 100 Hz
2.0
@Frequency 100 Hz
 2.0
@Frequency 1e+6 Hz
2.0
@Frequency 1e+6 Hz
Dielectric Strength 35.0 kV/mm889 kV/in
Dissipation Factor  0.00060
@Frequency 100 Hz
0.00060
@Frequency 100 Hz
 0.00060
@Frequency 1e+6 Hz
0.00060
@Frequency 1e+6 Hz
Comparative Tracking Index 300 V300 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C189 °F
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °F
Vicat Softening Point 90.0 °C194 °F50°C/hr/50 N
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
Oxygen Index 26 %26 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vestyron® 512 Impact-Modified Polystyrene
Vestyron® 640 Impact-Modified Polystyrene
Vestyron® 620 Impact-Modified Polystyrene
Vestyron® 527 S Impact-Modified Polystyrene
Vestyron® 516 Impact-Modified Polystyrene

PHUM74 / 47507

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.