MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) TEDUR® L 9217-7 PPS, 65% Glass/Mineral Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Base Polymer: Polyphenylene Sulfide

Filler/Additive System: 65% glass/mineral fibers

Special Features: High stiffness, hot oil resistant, hydrolysis resistant

Market Segment: Automotive, Machinery, Lighting

Typical Applications: Highly stressed parts

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.97 g/cc0.0712 lb/in³ISO 1183
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 140 MPa20300 psiISO 527
Elongation at Break 1.2 %1.2 %ISO 527
Tensile Modulus 19.0 GPa2760 ksiISO 527
Flexural Strength 240 MPa34800 psiISO 178
Flexural Modulus 19.0 GPa2760 ksiISO 178
Flexural Strain at Break 1.4 %1.4 %Flexural deflection at max force; ISO 178
Izod Impact, Unnotched (ISO) 25.0 kJ/m²11.9 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 278 °C532 °FISO 75-1/-2
Flammability, UL94 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
passed; DIN EN 60695
 
Processing PropertiesMetricEnglishComments
Melt Temperature 320 - 340 °C608 - 644 °FInjection molding
Mold Temperature >= 140 °C>= 284 °FInjection molding
Drying Temperature 130 - 140 °C
@Time 7200 - 14400 sec
266 - 284 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyphenylene Sulfide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) TEDUR® L 9217-7 S PPS, 65% Glass/Mineral Fiber Reinforced
Celanese FORTRON 6165A6 PPS, 65% Mineral / Glass Reinforced
Mocom (ALBIS) TEDUR® L 9220-1 Polyphenylene Sulphide, 65% Glass/Mineral Fiber Reinforced

PALBIS8347 / 242406

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.