MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Imerys Kaolex™ BN Kaolin
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Kaolex BN is a Hydrated Aluminum Silicate. It is an econoMical high surface area clay, well suited for use in roofing granules and refractory applications..

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.60 g/cc2.60 g/cc
Brightness 70 - 80 %70 - 80 %% Reflectance
Particle Size 0.30 µm0.30 µmaverage
Particle Mesh Size 325 Mesh325 Mesh0.4% retained
pH 4.5 - 5.54.5 - 5.5
Specific Surface Area 33 - 38 m²/g33 - 38 m²/g
Brookfield Viscosity 500 - 1000 cP
@Temperature 25.0 - 500 °C
500 - 1000 cP
@Temperature 77.0 - 932 °F
20 RPM, 70% clay/water slip
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 50000 ohm-cm50000 ohm-cmspecific resistance
 
Descriptive Properties
Colorwhite
Heating Loss (% max as produced)1at 105°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Imerys Afton™ Kaolin
CoorsTek ACI-Ni6 Tungsten Carbide
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
CIMBAR Suspengel™ 200 Plus High Purity Bentonite, Industrial Grade

CIMERY041 / 88391

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.