MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LATI LATILUB 87/28-15T K/30 Polycarbonate (PC), 15% PTFE, 30% Carbon Fiber Reinforced Self Lubricating Plastic  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon + PTFE Filled

Material Notes: Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intrinsic properties (moldability, low cost, lightness, high mechanical properties), low friction coefficient and low wear are required.

Specific Notes for this Material: polycarbonate base (PC); 15% PTFE; good wear resistance; low wear value even under load; 30% carbon fiber; high rigidity; high mechanical properties; low specific resistance.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ISO 1183
Water Absorption 0.10 %0.10 %at 23°C; ISO 62
Linear Mold Shrinkage 0.00080 cm/cm0.00080 in/inLATI
Linear Mold Shrinkage, Transverse 0.00080 cm/cm0.00080 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 100 MPa14500 psiISO 527
Flexural Modulus 10.25 GPa1487 ksiASTM D790
Izod Impact, Notched 0.600 J/cm
@Temperature 23.0 °C
1.12 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10000 ohm10000 ohmIEC 93
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 141 °C286 °FASTM D648
Vicat Softening Point 147 °C297 °F50°C/h 50N; ISO 306
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 100 - 120 °C212 - 248 °F
Drying Temperature 120 - 130 °C248 - 266 °FNecessary, temperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourNecessary, drying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)YIEC 335
Heat Resistance - Ball Test (165°C)NIEC 335
Injection Speedhigh
Needle Burner TestY1.47 mm
 Y3.05 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC FC 133 PTFE, 15% Carbon
BASF Ultrason® E 2010 C6 30% Carbon Filled
Aluminum A413.1 Composition Spec
RTP Company RTP 4299 X 117414 Thermoplastic Polyimide (TPI), Carbon Fiber
RTP Company RTP 4285 TFE 15 Thermoplastic Polyimide (TPI), Carbon Fiber - PTFE Lubricated

PLATI202 / 50200

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.