  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Chemical Advanced Materials Proteus™ LSG HDPE High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Life science grade HDPE stock shapes, pre-assessed for biocompatibility on both resin and stock shape for up to 24 hours body contact according to USP VI and ISO 10993, as well as wetted contact in bioprocessing. Exhibits low extractables and leaching, low moisture absorption, and great resistance to chemical cleaning agents, allowing parts to retain excellent impact resistance and good tensile strength throughout repeated use.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 63.063.0ISO 868
Tensile Strength 29.0 MPa4210 psiISO 527-1/-2 (7)
Elongation at Yield 9.00 %9.00 %ISO 527-1/-2 (7)
Flexural Strength 30.0 MPa4350 psiISO 178 (12)
Compressive Yield Strength  12.0 MPa
@Strain 1.00 %
1740 psi
@Strain 1.00 %
ISO 604 (10)
 18.0 MPa
@Strain 2.00 %
2610 psi
@Strain 2.00 %
ISO 604 (10)
 26.0 MPa
@Strain 5.00 %
3770 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 21.0 MPa3050 psiASTM D732
Charpy Impact, Notched 1.60 J/cm²7.61 ft-lb/in²Double Notched
 6.60 J/cm²31.4 ft-lb/in²ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C
@Temperature 23.0 - 100 °C
66.7 µin/in-°F
@Temperature 73.4 - 212 °F
Minimum Service Temperature, Air -100 °C-148 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents LimitedLimited
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SMU781 / 323895

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.