MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arya Sasol LFI 2575 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description: LFI2575 is a low density polyethylene, with good toughness and good biaxial shrink properties. This product is suitable for producing medium-duty films and containers and contains no-slip and anti-block additives that have low energy consumption during processing, good melt strength and a good drawdown ability. LFI2575 has been manufactured under SABTEC licensed technology.

Application: Blown film extrusion, surface protection films, lamination films

Forms: Pellets

Attribute: Good toughness, low blocking behavior

Additives: Antioxidant: Yes; Antiblock: No; Slip Agent: No

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ISO 1183
Thickness 45.0 - 100 microns1.77 - 3.94 mil
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.0 MPa1740 psiISO 527-1,3
Film Tensile Strength at Yield, TD 12.0 MPa1740 psiISO 527-1,3
Film Elongation at Break, MD >= 200 %>= 200 %ISO 527-1,3
Film Elongation at Break, TD >= 500 %>= 500 %ISO 527-1,3
Modulus of Elasticity 0.190 GPa27.6 ksiMD; ISO 527-1,3
 0.200 GPa29.0 ksiTD; ISO 527-1,3
Coefficient of Friction 0.700.70ASTM D1894
Tear Strength 30.0 kN/m171 pliTD; ISO 6383-2
 35.0 kN/m200 pliMD; ISO 6383-2
Dart Drop Total Energy 20.0 J/cm0.0375 ft-lb/milASTM D4272
Film Tensile Strength at Break, MD 28.0 MPa4060 psiISO 527-1,3
Film Tensile Strength at Break, TD 25.0 MPa3630 psiISO 527-1,3
 
Optical PropertiesMetricEnglishComments
Haze 50 %50 %ASTM D1003 A
Gloss 34 %34 %[GU], 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 190 °C347 - 374 °FExtruder temperature profile
Blow-up Ratio (BUR) 2.0 - 4.02.0 - 4.0
 
Descriptive Properties
Blocking<5 gASTM D3354
Re-blocking20 gSABTEC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARYA005 / 250459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.