MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Proto3000 – 3D Engineering Solutions

ASTM A36 Steel, bar
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Steel for general structural purposes including bridges and buildings.

Key Words: UNS K02600
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 400 - 550 MPa58000 - 79800 psi
Tensile Strength, Yield 250 MPa36300 psi
Elongation at Break 20 %20 %in 200 mm
 23 %23 %In 50 mm.
Modulus of Elasticity 200 GPa29000 ksi
Compressive Yield Strength 152 MPa22000 psiAllowable compressive strength
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.260.26
Shear Modulus 79.3 GPa11500 ksi
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.29 %0.29 %
Copper, Cu >= 0.20 %>= 0.20 %only if copper steel is specified
Iron, Fe 98 %98 %
Manganese, Mn 0.80 - 1.2 %0.80 - 1.2 %
Phosphorus, P 0.040 %0.040 %
Silicon, Si 0.15 - 0.40 %0.15 - 0.40 %
Sulfur, S 0.050 %0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A36 Steel, plate
ASTM A36 Steel, flange
AISI 1018 Steel, cold drawn
ASTM A572 Steel, grade 50
Aluminum 6061-T6; 6061-T651

MSA36A / 14015

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.