Ravago Manufacturing Americas Hylex® P1310G15 HB Polycarbonate, 15% Fiberglass Reinforced, UV Stabilized
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, 20% Glass Filled
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.
Information provided by Entec.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.30
g/cc
1.30
g/cc
ASTM D792
Water Absorption
0.14 %
0.14 %
24-Hr Immersion; ASTM D570
Linear Mold Shrinkage, Flow
0.0020
-
0.0040
cm/cm
0.0020
-
0.0040
in/in
ASTM D955
Melt Flow
5.0
-
9.0
g/10 min
@Load 1.20 kg,
Temperature 300 °C
5.0
-
9.0
g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
88
88
ASTM D785
Tensile Strength, Yield
97.0
MPa
14100
psi
ASTM D638
Elongation at Yield
5.0 %
5.0 %
ASTM D638
Flexural Strength
131
MPa
19000
psi
ASTM D790
Flexural Modulus
4.414
GPa
640.2
ksi
ASTM D790
Izod Impact, Notched
1.07
J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
2.00
ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
4.00e+16
ohm-cm
4.00e+16
ohm-cm
ASTM D257
Dielectric Strength
16.9
kV/mm
@Thickness 3.17 mm
430
kV/in
@Thickness 0.125 in
in air; ASTM D149
Arc Resistance
120
sec
120
sec
ASTM D495
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
149
°C
300
°F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
145
°C
293
°F
Unannealed; ASTM D648
Vicat Softening Point
160
°C
320
°F
ASTM D1525
Flammability, UL94
HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized
Entec Hylex® P1010FR Polycarbonate
Ravago Manufacturing Americas Hylex® P1010G10 HB Polycarbonate, 10% Fiberglass Reinforced
Clariant Renol PCSP0013WT-192 Polycarbonate, Flame Retardant, UV Stabilized, High Opacity
A. Schulman Diamond ASAPC 130 UV Stabilized
PENT056A / 36086
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.