MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
Categories: Polymer; Thermoplastic; Polybenzimidazole (PBI)

Material Notes: U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. Celazole PBI is ideal for applications where requirements cannot be met by other resins—in extreme high temperatures, in harsh chemical or plasma environments, or in applications where durability and wear resistance are important. Parts molded of Celazole PBI are being used in semiconductor and flat panel display manufacture, electrical insulating parts, heat insulating applications, as well as seals, bearings and wear plates in various industrial applications. They are also being evaluated in demanding aerospace applications requiring outstanding strength and short-term high temperature resistance.

Information provided by PBI Performance Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/cc
Water Absorption 0.40 %
@Temperature 22.8 °C,
Time 86400 sec
0.40 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 104104ASTM D785
Hardness, Rockwell M >= 125>= 125ASTM D785
Hardness, Shore D 9595ASTM D2240
Tensile Strength 160 MPa23200 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 5.90 GPa856 ksiASTM D638
Flexural Strength 220 MPa31900 psiASTM D790
Flexural Modulus 6.50 GPa943 ksi
Compressive Yield Strength 390 MPa56600 psiASTM D695
 340 MPa
@Strain 10 %
49300 psi
@Strain 10 %
ASTM D695
Compressive Modulus 5.90 GPa856 ksiASTM D695
Fatigue Strength 56.0 MPa
@Frequency 1 Hz,
# of Cycles 1.00e+6
8120 psi
@Frequency 1 Hz,
# of Cycles 1.00e+6
ASTM D638
Izod Impact, Notched 0.300 J/cm0.562 ft-lb/inASTM D256
Izod Impact, Unnotched 5.90 J/cm11.1 ft-lb/in
Coefficient of Friction, Dynamic 0.160.16Aluminum
 0.160.16Steel
 0.180.18Brass
Coefficient of Friction, Static 0.140.14Aluminum
 0.150.15Steel
 0.160.16Brass
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmASTM D257
Dielectric Constant  3.3
@Frequency 100000 Hz
3.3
@Frequency 100000 Hz
ASTM D150
 3.4
@Frequency 1000 Hz
3.4
@Frequency 1000 Hz
ASTM D150
 3.4
@Frequency 10000 Hz
3.4
@Frequency 10000 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm584 kV/inASTM D149
Dissipation Factor  0.0030
@Frequency 10000 Hz
0.0030
@Frequency 10000 Hz
ASTM D150
 0.034
@Frequency 100000 Hz
0.034
@Frequency 100000 Hz
ASTM D150
Arc Resistance 185 sec185 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.0 µm/m-°C
@Temperature 25.0 - 150 °C
12.8 µin/in-°F
@Temperature 77.0 - 302 °F
ASTM TMA
 33.0 µm/m-°C
@Temperature 200 - 300 °C
18.3 µin/in-°F
@Temperature 392 - 572 °F
ASTM TMA
Thermal Conductivity 0.403 W/m-K
@Temperature 25.0 °C
2.80 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 435 °C815 °FASTM D648
Glass Transition Temp, Tg 427 °C801 °FASTM DMA
Oxygen Index 58 %58 %ASTM D2863
 
Descriptive Properties
Environmental Resistance Ratings, ASTM D 543“Mobile Bay” SourgasNo effect after 7 days at 450°F
 “NACE “A”No effect after 7 days at 200°F
 5% Sodium HypochloriteNo effect after 1 day at 200°F
 5% Sodium HypochloriteSmall effect after 7 days at 200°F
 5% Sodium HypochloriteSmall effect after 30 days at 200°F
 Acetic Acid (10%)No effect after 1 day at 200°F
 Acetic Acid (10%)Small effect after 7 days at 200°F
 Acetic Acid (10%)Small effect after 30 days at 200°F
 Acetic Acid (Glacial)No effect after 7 days at 200°F
 Boiling Water, 212°FNo effect after 1 day
 Boiling Water, 212°FSmall effect after 7 days
 Boiling Water, 212°FSmall effect after 30 days
 BrineNo effect after 7 days at 200°F
 DimethylacetamideLarge effect after 1 day at 200°F
 DimethylacetamideSevere effect after 7 days at 200°F
 GasolineNo effect after 7 days at 200°F
 Hydrochloric Acid (10%)No effect after 1 day at 200°F
 Hydrochloric Acid (10%)Large effect after 7 days at 200°F
 Hydrochloric Acid (10%)Severe effect after 30 days at 200°F
 Hydrochloric Acid (37%)Small effect after 1 day at 200°F
 Hydrochloric Acid (37%)Large effect after 7 days at 200°F
 Hydrochloric Acid (37%)Severe effect after 30 days at 200°F
 KeroseneNo effect after 7 days at 200°F
 MethanolNo effect after 1 day
 MethanolNo effect after 7 days
 MethanolSmall effect after 30 days
 Methyl Ethyl KetoneNo effect after 7 days
 Methylene ChlorideNo effect after 7 days
 Monsanto Therminol-66 Heat Transfer FluidNo effect after 7 days at 520°F
 NACE “B”No effect after 7 days at 200°F
 Nitric Acid (10%)Small effect after 1 day at 200°F
 Nitric Acid (10%)Severe effect after 7 days at 200°F
 Nitric Acid (10%)Severe effect after 30 days at 200°F
 PhenolNo effect after 1 day at 200°F
 PhenolNo effect after 7 days at 200°F
 PhenolNo effect after 30 days at 200°F
 Phosphoric Acid (35%)No effect after 1 day at 200°F
 Phosphoric Acid (35%)Small effect after 7 days at 200°F
 Phosphoric Acid (35%)Severe effect after 30 days at 200°F
 Skydrol B HydraulicNo effect after 7 days at 200°F
 Sodium Carbonate (10%)No effect after 1 day at 200°F
 Sodium Carbonate (10%)No effect after 7 days at 200°F
 Sodium Carbonate (10%)No effect after 30 days at 200°F
 Sodium Hydroxide (Caustic 15%)No effect after 1 day at 200°F
 Sodium Hydroxide (Caustic 15%)Small effect after 7 days at 200°F
 Sodium Hydroxide (Caustic 15%)Large effect after 30 days at 200°F
 Steam, 650°F, 2200 psiSmall effect after 1 day
 Steam, 650°F, 2200 psiSmall effect after 7 days
 Steam, 650°F, 2200 psiSmall effect after 30 days
 Sulfuric Acid (30%)No effect after 1 day at 200°F
 Sulfuric Acid (30%)Large effect after 7 days at 200°F
 Sulfuric Acid (30%)Severe effect after 30 days at 200°F
 Texaco Havoline Supreme 30W Motor OilNo effect after 7 days at 200°F
 TolueneNo effect after 7 days
 Triethylene glycolNo effect after 1 day at 200°F
 Triethylene glycolNo effect after 7 days at 200°F
 Triethylene glycolNo effect after 30 days at 200°F
 Triethylene glycolNo effect after 1 day at 450°F
 Triethylene glycolNo effect after 7 days at 450°F
 Triethylene glycolNo effect after 30 days at 450°F
 XyleneNo effect after 7 days

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole
PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole
Mitsubishi Chemical Advanced Materials Duratron™ CU60 PBI Polybenzimidazole, unfilled, compression molded

PPBIP001 / 140555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.