MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes:

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0050 cm/cm0.0040 - 0.0050 in/inASTM D955
Melt Flow 11 g/10 min
@Load 8.70 kg,
Temperature 190 °C
11 g/10 min
@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.7 MPa3580 psiASTM D412
Tensile Modulus 2.07 GPa300 ksiASTM D412
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 75.6 °C168 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 210 °C380 - 410 °F
Mold Temperature 37.8 - 65.6 °C100 - 150 °F
Dry Time 2 - 4 hour
@Temperature 104 °C
2 - 4 hour
@Temperature 220 °F
to ensure moisture level is less than 0.02%
Injection Pressure 4.96 - 8.27 MPa720 - 1200 psiSecondary
 8.27 - 13.8 MPa1200 - 2000 psiInitial
Back Pressure 0.000 - 0.345 MPa0.000 - 50.0 psi
Shot Size 30 - 80 %30 - 80 %
Screw Speed 20 - 100 rpm20 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Huntsman IROGRAN® A 80 P 5039 TPU-Polyether
Overview of materials for Silicone Polyurethane, Ether Based
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced

PCLAR194 / 82319

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.