Description: Nylon N-277 is a 40% mineral reinforced, heat stabilized nylon 6/6 that provides excellent flatness and dimensional stability in injection molded parts. It is recommended for producing flat, low warp parts and readily fills complex shapesInformation provided by Celanese Corporation. |