MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Orion Performance Compounds i-On3D™ ABS CF20 Acrylonitrile Butadiene Styrene, 20% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled

Material Notes: 11-122-000-300

Description: i-On3D™ ABS CF20 is a specially formulated carbon fiber reinforced ABS compound for use in 3D printing applications. Excellent dimensional stability and printability useful in large format printing applications.

Features:

  • Low Warpage
  • Good Surface Finish
  • Good Interlayer Bonding
  • Dimensionally Stable
Applications:
  • Jigs & fixtures
  • Tooling
  • Complex parts
  • LFAM
Special Instructions: Avoid excessive drying. Lower dryer temps to 140F if expecting longer periods in dryer.

Information provided by Orion Performance Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 93.1 MPa13500 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Tensile Modulus 12.8 GPa1850 ksiASTM D638
Flexural Strength 143 MPa20800 psiASTM D790
Flexural Modulus 12.4 GPa1800 ksiASTM D790
Izod Impact, Notched 0.641 J/cm1.20 ft-lb/inASTM D265
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 3.00e+10 - 5.00e+10 ohm3.00e+10 - 5.00e+10 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C220 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 266 - 288 °C510 - 550 °F
Zone 1 246 - 266 °C475 - 510 °F
Zone 2 260 - 277 °C500 - 530 °F
Zone 3 260 - 277 °C500 - 530 °F
Melt Temperature 260 - 288 °C500 - 550 °F
Drying Temperature 93.3 °C200 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content >= 0.020 %>= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PORI9960 / 320651

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.