MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zoltek™ PX30 MF/ME Milled Carbon Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX30 High Purity Milled Fibers are 99+% pure carbon fibers derived from ZOLTEK’s high temperature batch graphitization process. All ZOLTEK milled products are free of any sizings. ZOLTEK’s in-house milling system ensures product quality and traceability from raw material through finished product.

APPLICATIONS: • RFI/EMI shielding of electronic devices • Buoyancy • Static dissipation • Resin-rich surface reinforcement in composites • Low-cost friction compounds.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.490 g/cc0.0177 lb/in³
Density 1.75 g/cc0.0632 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00170 ohm-cm0.00170 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 99 %99 %Approximate
 
Descriptive Properties
Fiber Diameter (µm)7.2
Fiber Length100 µm(MF150. Average)
 150 µm (MF200. Average)
Filament ShapeRound
Linear Resistivity (Omega;/cm)0.069

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 SW48-50 Woven Carbon Fiber Fabric
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric
Sinotek Materials Packing Carbon Fiber with Graphite
Zoltek™ PX35 UD900V Uni-Directional Carbon Fabric
Zoltek™ PX35 Continuous Tow Carbon Fiber

ECZO815 / 232283

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.