MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem BU004 Blow Molding High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Containers for lubricating oils, alcohol, cosmetics and yogurts; Toys.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.966 g/cc0.966 g/ccASTM D1505/D792
ESCR 100% Igepal® 32 hour
@Temperature 50.0 °C
32 hour
@Temperature 122 °F
h/50%f; compression molded 2 mm notched-plaques; ASTM D1683
ESCR 10% Igepal® 23 hour
@Temperature 50.0 °C
23 hour
@Temperature 122 °F
h/50%f; compression molded 2 mm notched-plaques; ASTM D1683
Melt Flow  0.38 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.38 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 32 g/10 min
@Load 21.6 kg,
Temperature 190 °C
32 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength at Break 29.0 MPa4210 psiASTM D638
Tensile Strength, Yield 33.0 MPa4790 psiASTM D638
2% Secant Modulus 1.36 GPa197 ksiASTM D790
Izod Impact, Notched 3.00 J/cm5.62 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C174 °FASTM D648
Vicat Softening Point 129 °C264 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BL2631 High Density Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
ExxonMobil AP60-007 High Density Polyethylene Resin
Global B-5200 High Density Polyethylene
Petromont 5001 High Density Polyethylene Resin

PBRAS712 / 109492

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.