MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HDP8660.29 Rotational Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes: Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance of low temperature toughness, creep resistance, stiffness, ESCR and tear properties.

Availability: Latin America, North America and South America

Additive:

  • Long Term UV-15 Stabilizer: Yes
Applications:
  • Industrial Products
  • Intermediate Bulk Containers
  • Large Agricultural Tanks
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 g/cc0.0340 lb/in³ASTM D4883
ESCR 100% Igepal® 550 hour550 hourASTM D1693 Condition A
ESCR 10% Igepal® 50 hour50 hourASTM D1693 Condition A
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psi2.0 in/min; ASTM D638
Elongation at Yield 20 %20 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 896 MPa130000 psiASTM D790
Impact Test  108 J
@Thickness 3.17 mm,
Temperature -40.0 °C
80.0 ft-lb
@Thickness 0.125 in,
Temperature -40.0 °F
ARM
 244 J
@Thickness 6.35 mm,
Temperature 25.0 °C
180 ft-lb
@Thickness 0.250 in,
Temperature 77.0 °F
ARM
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 °C264 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C153 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °C106 °FASTM D648
 
Descriptive Properties
FeaturesLong Term UV 8 Stabilization
Form35 US Mesh Powder

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HD 8660.29 Rotational Molding Resin
ICO Polymers ICORENE™ 150-1049 HDPE Rotational Molding Resin
ICO Polymers ICORENE™ 150-1119 HDPE Rotational Molding Resin
ICO Polymers ICORENE™ 150-1498 HDPE Rotational Molding Resin
LyondellBasell Lupolen 4021 K RM High Density Polyethylene (HDPE), Rotational Molding Grade

PEXB078 / 37383

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.