MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ensinger TECACOMP LCP LDS black 1014978 Liquid crystal polymer
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Unfilled

Material Notes:
  • developed for the LPKF-LDS® process
  • low thermal expansion
Target Industries:
  • automotive industry
  • electrical engineering
  • LED lighting technology
  • mechanical engineering
former material REZ-RS-4107

Information provided by Ensinger Inc.

Vendors: Ensinger TECACOMP compounds withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³
Water Absorption at Saturation <= 0.10 %<= 0.10 %50 % relative humidity up to saturation; DIN EN ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0030 cm/cm0.0030 in/inDIN EN ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 93.0 MPa13500 psiDIN EN ISO 527-1
Elongation at Break 1.3 %1.3 %DIN EN ISO 527-1
Modulus of Elasticity 10.5 GPa1520 ksiDIN EN ISO 527-1
Adhesive Bond Strength 9.10 MPa1320 psitest method: pull-off-test, (metal path)
Charpy Impact Unnotched 0.800 J/cm²3.81 ft-lb/in²DIN EN ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.80e+13 ohm-cm3.80e+13 ohm-cmDIN EN 61340-2-3
Surface Resistance 4.10e+12 ohm4.10e+12 ohmDIN EN 61340-2-3
Dielectric Constant 3.52
@Frequency 1e+9 Hz
3.52
@Frequency 1e+9 Hz
Dissipation Factor 0.0030
@Frequency 1e+9 Hz
0.0030
@Frequency 1e+9 Hz
Comparative Tracking Index 275 V275 VDIN EN 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  16.0 µm/m-°C
@Temperature 50.0 - 100 °C
8.89 µin/in-°F
@Temperature 122 - 212 °F
DIN EN ISO 11359-1;2
 25.0 µm/m-°C
@Temperature 100 - 150 °C
13.9 µin/in-°F
@Temperature 212 - 302 °F
DIN EN ISO 11359-1;2
 30.0 µm/m-°C
@Temperature 150 - 200 °C
16.7 µin/in-°F
@Temperature 302 - 392 °F
DIN EN ISO 11359-1;2
 34.0 µm/m-°C
@Temperature 200 - 250 °C
18.9 µin/in-°F
@Temperature 392 - 482 °F
DIN EN ISO 11359-1;2
CTE, linear, Transverse to Flow  32.0 µm/m-°C
@Temperature 50.0 - 100 °C
17.8 µin/in-°F
@Temperature 122 - 212 °F
DIN EN ISO 11359-1;2
 40.0 µm/m-°C
@Temperature 100 - 150 °C
22.2 µin/in-°F
@Temperature 212 - 302 °F
DIN EN ISO 11359-1;2
 49.0 µm/m-°C
@Temperature 150 - 200 °C
27.2 µin/in-°F
@Temperature 302 - 392 °F
DIN EN ISO 11359-1;2
 60.0 µm/m-°C
@Temperature 200 - 250 °C
33.3 µin/in-°F
@Temperature 392 - 482 °F
DIN EN ISO 11359-1;2
Specific Heat Capacity 1.25 J/g-°C0.299 BTU/lb-°FDIN EN 821
Thermal Conductivity 0.760 W/m-K5.27 BTU-in/hr-ft²-°Fthrough-plane; ISO 22007-4:2008
 1.61 W/m-K11.2 BTU-in/hr-ft²-°Fin-plane; ISO 22007-4:2008
Melting Point 320 °C608 °FDIN 53765
Maximum Service Temperature, Air 200 °C392 °Flong term
 260 °C500 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 274 °C525 °FISO-R 75 Method A
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
DIN IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 320 - 340 °C608 - 644 °FCylinder
Nozzle Temperature 350 °C662 °F
Zone 1 320 °C608 °F
Zone 2 325 °C617 °F
Zone 3 330 °C626 °F
Zone 4 340 °C644 °F
Melt Temperature 350 °C662 °FMaterial temperature
Mold Temperature 160 °C320 °F
Drying Temperature 150 °C302 °F
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hour
Moisture Content <= 0.10 %<= 0.10 %Permissible residual moisture content
Injection Pressure 150 MPa21800 psi
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
Back Pressure 0.100 - 0.300 MPa14.5 - 43.5 psi
 
Descriptive Properties
Colorblack
Injection ratefast
Laser Marking Parameter1.6-3.2 m/sForward movement
 100-200 KZFrequency
 2.5 WPower
Thermal diffusivity0.31 mm2/sthrough-plane, ISO 22007-4:2008
 0.93 mm2/sin-plane, ISO 22007-4:2008

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9000 / 318928

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.