MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 299 X 131299 A Nylon 6/6 (PA), Carbon Fiber - Glass Fiber - Impact Modified - Heat Stabilized - Electrically Conductive - Preliminary Datasheet
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Carbon Black + Glass Fiber Filled

Material Notes: Preliminary Data Sheet

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D 792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
@Thickness 3.17 mm
0.0030 - 0.0060 in/in
@Thickness 0.125 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 131 MPa19000 psiASTM D 638
Elongation at Break 2.5 - 3.5 %2.5 - 3.5 %ASTM D 638
Tensile Modulus 8.27 GPa1200 ksiASTM D 638
Flexural Strength 193 MPa28000 psiASTM D 790
Flexural Modulus 6.89 GPa1000 ksiASTM D 790
Izod Impact, Notched 0.587 J/cm
@Thickness 3.17 mm
1.10 ft-lb/in
@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 4.81 J/cm
@Thickness 3.17 mm
9.00 ft-lb/in
@Thickness 0.125 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 238 °C460 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 299 °C530 - 570 °F
Mold Temperature 65.6 - 107 °C150 - 225 °F
Drying Temperature 79.4 °C
@Time 14400 sec
175 °F
@Time 4.00 hour
Moisture Content 0.20 %0.20 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 124 MPa10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics Duracon® CH-10 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
RTP Company ESD 283 TFE 5 HS Nylon 6/6 (PA); Carbon Fiber - Electrically Conductive - PTFE Lubricated - Heat Stabilized
Solvay THORNEL® VMX-24 Pitch-Based Fiber
Polyram RamShine PV3003R2 Acrylonitrile Butadiene Styrene, 10% Carbon Fiber
Oxford Polymers 30CF 30% Carbon Fiber Reinforced Polyphenylene Sulfide

PQZTA23924 / 159266

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.