MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco AFP White Oil
Categories: Fluid; Lubricant; White Mineral Oil (WMO)

Material Notes: Chevron White Oil AFP is a technical grade white oil processed from paraffinic oil

Applications

Chevron White Oil AFP’s major application is the dedusting of animal feeds and the preparation of animal feed cubes and pellets.

Other applications for Chevron White Oil AFP include:

  • defoamer
  • mold release lubricant
  • component in the manufacture of plastic food containers

Key Words: CPS Number: 231039; MSDS Number: 7824
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 36 °36 °
Saybolt Viscosity at 100°F 72 SUS72 SUS
Kinematic Viscosity at 40°C (104°F) 13.2 cSt13.2 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -12.0 °C10.4 °FASTM D97
Flash Point 182 °C360 °FASTM D92
 
Descriptive Properties
Color+25, Saybolt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 1400 Antifoam
Dow 1410 ANTIFOAM
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil AD
ChevronTexaco Aero 50/Grade 100 Engine Oil AD Uncompounded

WCHEV132 / 74747

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.