MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo Plexiglas® VS-UVT Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, High Flow, Molded

Material Notes: Plexiglas® VS-UVT is a thermoplastic impact-modified acrylic resin suitable for injection molding. It is a high flow resin designed to provide exceptional UV transmission and excellent transparency making it an outstanding choice for in-vitro diagnostic applications.

Appearance: Clear/Transparent

Characteristics: Bondability; BPA Free; High Clarity; High Flow; Good Moldability

Applications: Medical/Healthcare Applications; Medical Appliances

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Water Absorption 0.30 %0.30 %24 hr. immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inASTM D955
Melt Flow 27 g/10 min
@Load 3.80 kg,
Temperature 230 °C
27 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8484ASTM D785
Tensile Strength, Ultimate 64.8 MPa9400 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 2.90 GPa420 ksiASTM D638
Flexural Strength <= 96.5 MPa<= 14000 psiASTM D790
Flexural Modulus 2.96 GPa430 ksiASTM D790
Izod Impact, Notched 0.160 J/cm0.300 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.187 W/m-K1.30 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 80.6 °C177 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.1 °C169 °Fannealed; ASTM D648
Vicat Softening Point 81.1 °C178 °F50°C/hr; 50N; ASTM D1525
 87.2 °C189 °F50°C/hr; 10N; ASTM D1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49
@Temperature 22.8 °C
1.49
@Temperature 73.0 °F
ND; ASTM D542
Haze <= 1.0 %
@Thickness 3.17 mm
<= 1.0 %
@Thickness 0.125 in
ASTM D1003
Transmission, Visible 92 %
@Thickness 3.17 mm
92 %
@Thickness 0.125 in
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Solarkote™ A200 Acrylic
Trinseo Plexiglas® Diffuse™ V045-68207 Acrylic Resin
Overview of materials for Acrylic, Optical Sheet
Trinseo Plexiglas® V920 Acrylic
Overview of materials for Acrylic, Heat Resistant, Molded

PARKG034 / 24388

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.