MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Aclo Accutech TPO TPO030T9V Paintable Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); TPO

Material Notes: Approved to Suzuki Spec Black B14257

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.965 g/cc0.0349 lb/in³ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inMD; ASTM D955
Linear Mold Shrinkage, Transverse 0.0105 cm/cm0.0105 in/inTD
Melt Flow 35 g/10 min35 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength, Yield 20.0 MPa2900 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Tensile Modulus 1.350 GPa195.8 ksiASTM D638
Flexural Strength 29.0 MPa4210 psiASTM D790
Izod Impact, Notched 0.534 J/cm
@Temperature -30.0 °C
1.00 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Heat Distortion 210250 %210250 %ASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.0 µm/m-°C
@Temperature 20.0 °C
37.2 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daplen™ AK4504 TPO Compound
Teknor Apex Telcar® TL-2651A Thermoplastic Elastomer
Borealis Daplen™ ED135AI TPO Compound
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade

PACLO094 / 22349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.