MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ASTM A27 Grade U-60-30 Cast Carbon Steel
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Carbon Steel Castings for General Application.

Key Words: 415-205, J02500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 460 MPa66700 psi
Tensile Strength, Yield 230 MPa33400 psi
Elongation at Break 25 %25 %
Reduction of Area 34 %34 %
Modulus of Elasticity 190 GPa27600 ksi
Poissons Ratio 0.290.29
Fatigue Strength 170 MPa24700 psi
Shear Modulus 73.0 GPa10600 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000213 ohm-cm0.0000213 ohm-cmequal weight 8.1 % IACS
 0.0000246 ohm-cm0.0000246 ohm-cmequal volume 7 % IACS
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 250 J/g108 BTU/lb
CTE, linear 12.0 µm/m-°C6.67 µin/in-°F
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°F
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°F
Melting Point 1420 °C2590 °Fsolidus
 1460 °C2660 °Fliquidus
Maximum Service Temperature, Air 400 °C752 °Fmax mechanical
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.25 %<= 0.25 %
Iron, Fe 98.1 - 100 %98.1 - 100 %
Manganese, Mn <= 0.75 %<= 0.75 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si <= 0.80 %<= 0.80 %
Sulfur, S <= 0.060 %<= 0.060 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MASTMA27E / 313984

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.