MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

American Elements Magnesium Nanoparticles
Categories: Metal; Nonferrous Metal; Magnesium Alloy; Pure Element

Material Notes: General Description

Magnesium (Mg) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Magnesium Particles are typically 20-60 nanometers (nm) with specific surface area (SSA) in the 30 – 70 m 2 /g range. Nano Magnesium Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Magnesium nanocrystals generally involve the potential to strengthen magnesium metal by adding them in order to create a lighter alloy competitive with aluminum and thereby increase the performance and energy efficiency of automobiles, airplanes and other vehicles and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications.

Key Words: Formula: Mg; CAS Number: 7439-95-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.738 g/cc0.06279 lb/in³
Particle Size 0.020 - 0.060 µm0.020 - 0.060 µm
Specific Surface Area 30 - 70 m²/g30 - 70 m²/g
Molecular Weight 24.31 g/mol24.31 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 650 °C1200 °F
Boiling Point 1090 °C1990 °F
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium, Mg; Sand Cast
Magnesium, Mg; Hard-Rolled Sheet
Overview of materials for Magnesium Alloy
Magnesium AM100A-T4, Cast
Magnesium AM20-F, Die Cast

EJAMER52 / 5535

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.