Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C. Industry: Paint & Coatings Uses: Architectural Coatings, Industrial Coatings, Flat/Matte, Satin, E-Coat, Powder Coatings, Pigmented Coatings Information provided by KaMin LLC. |