MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Description

Polyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Melt Flow 0.80 g/10 min0.80 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.0 MPa4060 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Flexural Strength 42.0 MPa6090 psiASTM D790
Flexural Modulus 2.20 GPa319 ksiASTM D790
Izod Impact, Notched 3.25 J/cm6.09 ft-lb/inASTM D256
Gardner Impact 29.0 J21.4 ft-lbASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene
A. Schulman TPP20AN05BK 20% Talc Filled, Heat Stabilized, Copolymer Polypropylene
Aclo Accutech Polypropylene Copolymer CP0436T20L Talc Reinforced
A. Schulman Fiberfil® PP-61/TC/20 Polypropylene Copolymer, 20% Talc

PASHU151 / 25115

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.