MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

COI Ceramics SiC Hollow Spheres
Categories: Ceramic; Carbide

Material Notes: Description: COI Ceramics, Inc. can fabricate a variety of thin shell hollow spheres of various compositions and sizes. These products are called Holospheres. They are available as loose spheres that can be added to a variety of end-user products. The spheres can also be bonded together and machined into products that are useful for various applications, or they may be bonded to other materials to produce hybrid articles.

Applications: Include thermal barrier layers for combustor liners, structural insulation for thermal protection systems, or structural cores in combination with CMCs to create engineered components.

Information from COI Ceramics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 100 microns3.94 milTypical Wall Thickness
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 1600 °C2910 °F
 
Descriptive Properties
Standard Sizes (mm)4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Erbslöh Aluminium DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6
Erbslöh Aluminium DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F
Erbslöh Aluminium DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F
Erbslöh Aluminium DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6
Erbslöh Aluminium DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F

CCOIC010 / 122050

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.