MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: PELLETHANE® 2103-90AEF elastomer is a polytetramethylene glycol ether based polyurethane elastomer, featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to attack by microorganisms. Its typical applications include wire and cable jacketing, wheels, film, tubing, and belting.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³
Linear Mold Shrinkage 0.012 cm/cm0.012 in/in
Melt Flow 3.0 g/10 min
@Load 8.70 kg,
Temperature 190 °C
3.0 g/10 min
@Load 19.2 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090
Tensile Strength at Break 37.9 MPa5500 psi
Elongation at Break 500 %500 %
50% Modulus 6.34 MPa
@Strain 50 %
6.34 MPa
@Strain 50 %
100% Modulus 8.96 MPa
@Strain 100 %
1300 psi
@Strain 100 %
300% Modulus 17.2 MPa
@Strain 300 %
2490 psi
@Strain 300 %
Secant Modulus 0.0690 GPa10.0 ksi2% Secant Modulus
Tear Strength 134 kN/m765 pli
Taber Abrasion, mg/1000 Cycles 5050H22 Wheel
Compression Set  25 %
@Temperature 23.0 °C
25 %
@Temperature 73.4 °F
 40 %
@Temperature 70.0 °C
40 %
@Temperature 158 °F
Tensile Set 60 %60 %Elongation set after break
 
Thermal PropertiesMetricEnglishComments
CTE, linear 156 µm/m-°C
@Temperature 20.0 °C
86.7 µin/in-°F
@Temperature 68.0 °F
Vicat Softening Point 102 °C216 °F
Glass Transition Temp, Tg -27.0 °C-16.6 °F
Clash Berg Stiffness Temperature 6.11 °C43.0 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer
Dow PELLETHANE® 2101-85A Polyurethane Elastomer (Ether-Ether Hybrid)

PDW274 / 34442

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.